Cad é 440 Cruach Dhosmálta?

Feb 24, 2026

Fág nóta

904L Stainless Steel Sheet for Chemical Processing EquipmentWhat is the main compositional difference between 201 and 304 stainless steelStainless Steel - Grade 409 (UNS S40900)

Ábhar Coibhéiseach de 440 Pláta Cruach Dhosmálta

440A Cruach Dhosmálta:

Coibhéiseach le AISI 440A, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 58812, MILS-AE (51440A)

Gráid chosúla: 7Cr17, 7Cr17MoV, X70CrMo15

440B Cruach Dhosmálta:

Coibhéiseach le AISI 440B, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5631, AMS 5632, AMS 5633, AMS 5634, AMS 5880, MILS-AE (51440B)

Gráid chosúla: 9Cr18, 9Cr18Mo, X90CrMoV18

440C Cruach Dhosmálta:

Comhionann le AISI 440C, ASTM A276, ASTM A314, ASTM A473, ASTM A580, ASTM A756, ASTM A580, AMS 5630, AMS 5880, MIL-S-862, SAE J405 (51440C)

Gráid chosúla: 9Cr18MoV, X105CrMo17

440 Comhdhéanamh Ceimiceach Pláta Cruach Dhosmálta(%)

Grád C Si Mn S P Cr Ni Mo
440A 0.60~0.75 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 0.030

Níos lú ná nó cothrom le 0.040

16.00-18.00 – Níos lú ná nó cothrom le 0.75
440B 0.85-0.95 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 0.030 Níos lú ná nó cothrom le 0.035 16.00-18.00 Níos lú ná nó cothrom le 0.60 Níos lú ná nó cothrom le 0.75
440C 0.95 – 1.20 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 1 Níos lú ná nó cothrom le 0.030 Níos lú ná nó cothrom le 0.040 16.00-18.00 – Níos lú ná nó cothrom le 0.75

Airíonna Meicniúla

Maoin 440A 440B 440C
Cruas (Rockwell C) 56-59 HRC 57-60 HRC 58-62 HRC
Neart Teanntachta (MPa) 760-820 760-840 760-820
Neart Teanntachta (MPa) 450-600 450-600 450-600
Fadú ag Sos (%) 20-25 15-20 10-15
Modal Leaisteachais (GPa) 200 200 200

Airíonna Fisiceacha

Maoin 440A 440B 440C
Dlús (g/cm³) 7.65 7.75 7.75
Seoltacht Theirmeach (W/m·K) 24 24 24
Saintoilleadh Teasa (J/kg·K) 460 460 460
Friotaíocht Leictreach (μΩ·cm) 60 60 60
Comhéifeacht an Leathnaithe Theirmeach (μm/m·K) 10.4 10.4 10.4

 

Glaoigh Linn