Comhdhéanamh Ceimiceach
| 1.4006 Cruach | GA 10088-3:2005 |
|---|---|
| Eilimint Cheimiceach | % i láthair |
| Carbón (C) | 0.08 - 0.15 |
| Cróimiam (Cr) | 11.50 - 13.50 |
| sileacain (Si) | 0.0 - 1.00 |
| Mangainéis (Mn) | 0.0 - 1.50 |
| fosfar (P) | 0.0 - 0.04 |
| Sulfar (S) | 0.0 - 0.02 |
| Nicil (Ni) | 0.0 - 0.75 |
| Iarann (Fe) | Iarmhéid |
Airíonna
| Maoin Fhisiciúil | Luach |
|---|---|
| Dlús | 7.75 g / cm³ |
| Leathnú Teirmeach | 9.9 x 10-6/K |
| Modal Leaisteachas | 300 GPa |
| Seoltacht Theirmeach | 24.9 W/m.K |
| Friotaíocht Leictreach | 0.57 x 10-6Ω.m |
| Barra - Suas le 160mm Dia nó Tiús | GA 10088-3:2005 |
|---|---|
| Maoin Mheicniúil | Luach |
| Strus Cruthúnas | 450 Nóiméad MPa |
| Neart Teanntachta | 650 - 850 MPa |
| Fadú A | 15 nóim % |