Tábla 1 .Raonta comhdhéanamh do 316 grád de steels dhosmálta.

Grád   C Mn Si P S Cr Mo Ni N
316 Min - - - 0 - 16.0 2.00 10.0 -
uas 0.08 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316L Min - - - - - 16.0 2.00 10.0 -
uas 0.03 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316H Min 0.04 0.04 0 - - 16.0 2.00 10.0 -
uas 0.10 0.10 0.75 0.045 0.03 18.0 3.00 14.0 -

 

Airíonna Meicniúla

Tábla 2 .Airíonna meicniúla cruach dhosmálta 316 grád.

Grád Str teanntachta (MPa) min Yield Str 0.2% Cruthúnas (MPa) min Elong (% i 50 mm) min Cruas
Rockwell B (HR B) max Brinell (HB) max
316 515 205 40 95 217
316L 485 170 40 95 217
316H 515 205 40 95 217

 

Tabhair faoi deara: Tá ceanglas ag 316H freisin maidir le méid gráin ASTM no. 7 nó níos garbh.

Airíonna Fisiceacha

Tábla 3 .Airíonna fisiceacha tipiciúla do steels dhosmálta 316 grád.

Grád Dlús(kg/m3) Modal Leaisteacha (GPa) Comh-éifeacht an Leathnaithe Teirmeach (µm/m/ céim ) Seoltacht Theirmeach (W/mK) Teas Sonrach 0-100 céim (J/kg.K) Friotaíocht Leictreach (nΩ.m)
0-100 céim 0-315 céim 0-538 céim Ag 100 céim Ag 500 céim
316/L/H 8000 193 15.9 16.2 17.5 16.3 21.5 500 740