Cairt Meáchan Píopa Cruach Dhosmálta ASTM A312
Jun 03, 2026
Fág nóta
Cad a chiallaíonn an “S” sa Sceideal (m.sh., SCH 40S)?
In ASTM A312/ANSI B36.19, seasann an "S" do sceidil cruach dhosmálta (5S, 10S, 40S, 80S) is minic a bhíonn tiús bhalla éagsúil ná sceidil cruach carbóin (a leanann ANSI B36.10). Mar shampla, d'fhéadfadh píopa cruach carbóin SCH 40 a bheith níos tiús nó níos tanaí ná píopa cruach dhosmálta SCH 40S ag brath ar an NPS.
Cad iad na lamháltais tiús bhalla do ASTM A312?
De réir ASTM A312, ní athróidh tiús an bhalla ag pointe ar bith níos mó ná:
Thar:20.0% de thiús balla ainmniúil.
Faoi:12.5% de thiús balla ainmniúil.
Cad é an fhoirmle chun meáchan Píopa Cruach Dhosmálta ASTM A312 a ríomh?
Le haghaidh ríomh láimhe tapa, is féidir leat an fhoirmle seo a leanas a úsáid:
Méadrach ( kg/m ): Meáchan (kg/m)=(OD - WT) * WT * 0.02491
Impiriúil (lb/ft): Meáchan (lb/ft)=(OD - WT) * WT * 10.69
(Cá háit a bhfuil OD=Trastomhas Lasmuigh i mm/orlach agus WT=Tiús Balla i mm/orlach)
Cairt Meáchan Píopa Cruach Dhosmálta ASTM A312
Tá meáchain bunaithe ar dhlús cruach dhosmálta (thart ar. 7.93 g/cm³ do TP304 agus 7.98 g/cm³ do TP316).
| NPS (Inse) | Trastomhas Lasmuigh (mm) | Sceideal (SCH) | Tiús Balla (mm) | Meáchan ( kg/m ) | Meáchan (lb/ft) |
| 1/2" | 21.34 | 10S | 2.11 | 1.02 | 0.69 |
| 1/2" | 21.34 | 40S | 2.77 | 1.29 | 0.87 |
| 3/4" | 26.67 | 10S | 2.11 | 1.30 | 0.87 |
| 3/4" | 26.67 | 40S | 2.87 | 1.71 | 1.15 |
| 1" | 33.40 | 10S | 2.77 | 2.13 | 1.43 |
| 1" | 33.40 | 40S | 3.38 | 2.55 | 1.71 |
| 1-1/2" | 48.26 | 10S | 2.77 | 3.16 | 2.12 |
| 1-1/2" | 48.26 | 40S | 3.68 | 4.12 | 2.77 |
| 2" | 60.33 | 10S | 2.77 | 4.00 | 2.69 |
| 2" | 60.33 | 40S | 3.91 | 5.53 | 3.72 |
| 3" | 88.90 | 10S | 3.05 | 6.57 | 4.41 |
| 3" | 88.90 | 40S | 5.49 | 11.47 | 7.71 |
| 4" | 114.30 | 10S | 3.05 | 8.51 | 5.72 |
| 4" | 114.30 | 40S | 6.02 | 16.35 | 10.99 |
Conas atá "Méid Ainmniúil Píobáin" (NPS) difriúil ó "Trastomhas Lasmuigh" (OD)?
I gcás píopaí faoi 14 orlach, ní mheaitseálann an NPS an OD iarbhír (m.sh., tá OD de 2.375" nó 60.33mm ag píopa 2 ").
I gcás píopaí 14 orlach agus níos mó, tá an NPS díreach comhionann leis an OD.
Caoinfhulaingt Píopaí Cruach ASTM A312
Caoinfhulaingt Trastomhas ASTM A312, lamháltais tríthoiseach astm a312
| NPS | ASTM A312/ASME SA312 Caoinfhulaingt OD | |||
| + | – | |||
| orlach | mm | orlach | mm | |
| 1/8 go 1 1 /2 >1 1 /2 go 4 >4 go 8 >8 go 18 >18 go 26 >26 go 34 >34 go 48 |
1/64(0.015) 1/32(0.031) 1/16(0.062) 3/32(0.093) 1/8(0.125) 5/32(0.156) 3/16(0.187) |
0.4 0.8 1.6 2.4 3.2 4.0 4.8 |
1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) |
0.8 0.8 0.8 0.8 0.8 0.8 0.8 |
Cad é na toisí do phíobán cruach dhosmálta ASTM A312?
Tá na sonraíochtaí tríthoiseach do phíobáin déanta as cruach dhosmálta ASTM A312 á rialú ag caighdeáin ASME B36.10 agus ASME B36.19. Cuimsíonn a raon Méid Ainmniúil Píobáin (NPS) ó chúpla orlach suas go dtí 30 orlach (le trastomhais lasmuigh idir 10.3 mm agus 762 mm), agus sainmhínítear tiús bhalla de réir Sceidil mar 5S, 10S, 40S, agus 80S.
Cairt Toisí do Phíopa Cruach Dhosmálta ASTM A312 (ASME B36.19)
| NPS (Inse) | DN (mm) | Trastomhas Lasmuigh (OD) (mm) | SCH 5S (WT mm) | SCH 10S (WT mm) | SCH 40S (WT mm) | SCH 80S (WT mm) |
| 1/8" | 6 | 10.29 | 1.00 | 1.24 | 1.73 | 2.41 |
| 1/4" | 8 | 13.72 | 1.20 | 1.65 | 2.24 | 3.02 |
| 3/8" | 10 | 17.15 | 1.20 | 1.65 | 2.31 | 3.20 |
| 1/2" | 15 | 21.34 | 1.65 | 2.11 | 2.77 | 3.73 |
| 3/4" | 20 | 26.67 | 1.65 | 2.11 | 2.87 | 3.91 |
| 1" | 25 | 33.40 | 1.65 | 2.77 | 3.38 | 4.55 |
| 1-1/4" | 32 | 42.16 | 1.65 | 2.77 | 3.56 | 4.85 |
| 1-1/2" | 40 | 48.26 | 1.65 | 2.77 | 3.68 | 5.08 |
| 2" | 50 | 60.33 | 1.65 | 2.77 | 3.91 | 5.54 |
| 2-1/2" | 65 | 73.03 | 2.11 | 3.05 | 5.16 | 7.01 |
| 3" | 80 | 88.90 | 2.11 | 3.05 | 5.49 | 7.62 |
| 4" | 100 | 114.30 | 2.11 | 3.05 | 6.02 | 8.56 |
| 5" | 125 | 141.30 | 2.77 | 3.40 | 6.55 | 9.53 |
| 6" | 150 | 168.28 | 2.77 | 3.40 | 7.11 | 10.97 |
| 8" | 200 | 219.08 | 2.77 | 3.76 | 8.18 | 12.70 |
| 10" | 250 | 273.05 | 3.40 | 4.19 | 9.27 | 12.70* |
| 12" | 300 | 323.85 | 3.96 | 4.57 | 9.53 | 12.70* |
Cad é an difríocht idir ASME B36.19 agus B36.10?
B36.19: Cruthaithe go sonrach le haghaidh Cruach Dhosmálta. Tá tiús ballaí níos éadroime aige (cosúil le SCH 5S agus 10S) chun costais a shábháil, toisc go bhfuil cruach dhosmálta níos láidre agus níos resistant- ná cruach carbóin.
B36.10: An caighdeán le haghaidh Cruach Charbóin agus píopaí iarann saoirsithe. Cé go bhforluíonn go leor toisí (cosúil le SCH 40 agus 40S), cuimsíonn B36.10 sceidil balla i bhfad níos troime (SCH 100, 120, 140, 160).
An bhfuil difríocht meáchain idir TP304 agus TP316?
Tá an difríocht diomaibhseach maidir le ríomhanna caighdeánacha, Cé go bhfuil TP316 beagán níos dlúithe (thart ar. 8,000 kg/m ³) ná TP304 (thart ar. 7,930 kg/m ³) mar gheall ar an ábhar moluibdín, úsáideann an caighdeán tionscail na fachtóirí meáchain céanna don dá i bhformhór na gcairteacha tráchtála.
Déantúsaíocht Píobán Cruach Dhosmálta ASTM A312 TP316/316L
Coinnímid stoc réidh d'ábhair chaighdeánacha sonraíochta (SCH 10S, SCH 40S) TP304 agus TP316, rud a chinntíonn loingsiú láithreach laistigh de 7 go 15 lá.
Chomh maith le píobaireacht, soláthraímid raon cuimsitheach feisteas comhlántach do phíobáin-lena n-áirítear feisteas, uillinn agus tíonna- atá deartha chun cabhrú le cliaint a bpróisis soláthair a shruthlíniú agus deireadh a chur leis na castachtaí deacra a bhaineann le comhpháirteanna éagsúla a aimsiú ina n-aonar.


Píob Cruach Dhosmálta ASTM A312 TP316/316L
Soláthraímid Deimhnithe Tástála Ábhar (MTCanna) iomlána a chomhlíonann caighdeáin EN 10204 3.1 nó 3.2. Is féidir cigireachtaí tríú páirtí (ag SGS, BV, TUV, Lloyd's) a shocrú, lena n-áirítear tástáil neamh-millteach (UT/ET), tástáil hidreastatach, tástáil creimthe idirghráinneach, agus go leor eile.


Glaoigh Linn