Pláta Cruach Dhosmálta 904L - Rollta Te (UNS N08904 / 1.4539)

Feb 24, 2026

Fág nóta

ASTM B673 Stainless Steel 904L Seamless Pipe304/304L Stainless SteelUNS N08904 / EN 1.4539 Stainless Steel Sheet Data Sheet

Sonraíocht Pláta Cruach Dhosmálta 904L Hot Rolled

Grád: 904L (UNS N08904)

Tiús: 1.2mm~200mm

Leithead: 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Fad: 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Werkstoff Uimh.: 1.4539

Caighdeán: ASTM A240, ASTM A959, ASTM B625. ASME SA-240, ASME SB-625. EN 10088-2, EN 10028-7, etc.

Bunús: TISCO, BAOSTEEL, POSCO, etc.

 

Ábhar Coibhéiseach de Pláta Cruach Dhosmálta 904L

Áirítear ar na hábhair choibhéiseacha de phláta cruach dhosmálta 904L i gcaighdeáin agus gráid éagsúla:

UNS: N08904

GA: 1.4539

DIN: X1NiCrMoCu25-20-5

AFNOR: Z2NCDU25-20

BS: 904S13

JIS: SUS 890L

Comhdhéanamh Ceimiceach Pláta Cruach Dhosmálta 904L(%)

Is gnách go dtagann comhdhéanamh ceimiceach plátaí Cruach Dhosmálta 904L laistigh de na raonta céatadáin seo a leanas:

C Cr Ni Mo Mn Si P S Cu Fe
Níos lú ná nó cothrom le 0.02% 19.0 – 23.0% 23.0 – 28.0% 4.0 – 5.0% Níos lú ná nó cothrom le 2.00% Níos lú ná nó cothrom le 1.00% Níos lú ná nó cothrom le 0.045% Níos lú ná nó cothrom le 0.035% 1.0 – 2.0% Iarmhéid