410 Táirgí Cruach Dhosmálta
Mar 23, 2026
Fág nóta



Comhdhúile Ceimiceacha
|
Eilimint |
C |
Mn |
Si |
Cr |
Ni |
P |
S |
Fe |
|---|---|---|---|---|---|---|---|---|
| Raon Comhdhéanaimh (%) | 0.08 – 0.15 | 1.00 max | 1.00 max | 11.50 – 13.50 | 0.75 max | 0.04 uas | 0.03 max | Iarmhéid |
Airíonna Meicniúla
|
Maoin Mheicniúil |
Luach (Méadrach) |
Luach (Imperial) |
|---|---|---|
| Neart Teanntachta | 480 – 620 MPa | 70 – 90 ksi |
| Neart Toradh | 275 – 450 MPa | 40 – 65 ksi |
| Cruas Brinell (HB) | 170 – 201 HB | 170 – 201 HB |
| Cruas Rockwell (HRC) | 20 – 30 HRC | 20 – 30 HRC |
| Cruas Vickers (HV) | 180 - 230 HV | 180 - 230 HV |
| Fadú | 20% – 25% | 20% – 25% |
| Modal Leaisteacha | 200 GPa | 29 x 10³ ks |
Glaoigh Linn