What is 1.4565 Stainless Steel?What is 1.4523 Stainless Steel?What is 1.4537 Stainless Steel?

Tiúsanna atá ar fáil do Alloy 316/316L:

3/16" 1/4" 5/16" 3/8" 7/16" 1/2" 9/16" 5/8" 3/4" 7/8" 1" 1 1/8"
4.8mm 6.3mm 7.9mm 9.5mm 11.1mm 12.7mm 14.3mm 15.9mm 19mm 22.2mm 25.4mm 28.6mm
1 1/4" 1 3/8" 1 1/2" 1 5/8" 1 3/4" 2" 2 1/4" 2 1/2" 2 3/4" 3" 3 1/4" 3 1/2"
31.8mm 34.9mm 38.1mm 41.3mm 44.5mm 50.8mm 57.2mm 63.5mm 69.9mm 76.2mm 82.6mm 88.9mm
3 3/4" 4" 4 1/4" 4 1/2" 4 3/4" 5" 5 1/4" 5 1/2" 5 3/4" 6"    
95.3mm 101.6mm 108mm 114.3mm 120.7mm 127mm 133.4mm 139.7mm 146.1mm 152.4mm    

 

Anailís Cheimiceach

Meáchan % (is uasluach na luachanna go léir mura sonraítear a mhalairt de raon)

Eilimint 316 316L
Cróimiam 16.0 min.-18.0 max. 16.0 min.-18.0 max.
nicil 10.0 min.-14.0 max. 10.0 min.-14.0 max.
moluibdín 2.00 min.-3.00 max. 2.00 min.-3.00 max.
Carbón 0.08 0.030
Mangainéis 2.00 2.00
Fosfar 0.045 0.045
Sulfair 0.03 0.03
sileacain 0.75 0.75
Nítrigin 0.1 0.1
Iarann Iarmhéid Iarmhéid

 