304H Bileog Cruach Dhosmálta

Mar 10, 2026

Fág nóta

Stainless Steel Grade 904L - Super Austenitic Anti-CorrosionStainless Steel Grade 309S - High Temp Alloy Steel GradeUNS S31635 Stainless Steel Knowledge

Caighdeán

ASME SA240, ASTM A240 / A240M

Grád

1.4948, S30409, SUS 304H, X7CrNi18-9

Fad

2000mm-6000mm (78.7''-236.2''), Saincheaptha

Leithead

1000mm-1500mm (39.4''-59''), Saincheaptha

Tiús

0.5mm-100mm (0.02''-3.94''), Saincheaptha

Críochnaigh Dromchla

2B, 2D, 8K, BA, Brushed, Checkered, Saincheaptha, Cabhraithe, Eitseáil, Líne Gruaige, Scáthán, Uimh.1, Uimh.4, Uimh.8, Gaineamh Blast

Teicníc

Annealing, Lúbthachta, Fuarrollta, Gearradh, Te Rolling

Foirm

Bileoga Brushed, Bileoga Seiceáilte, Cornaí, Bileoga Fuarrollta, Saincheaptha, Bileoga Cabhraithe, Bileoga Maol, Scragall, Bileoga Galbhánaithe, Bileoga Te Rollaithe, Bileoga Scáthán, Bileoga bréifnithe, Plátaí, Bileoga Snasta, Stiallacha

 

Téarmaí Gnó

Téarmaí Sonraíocht
Cainníocht Ordú Íosta: 5 Tonna
Praghas: Le hidirbheartú
Sonraí Pacáistithe:

Mar a Iarrtar

Am Seachadta: Laistigh de 7-10 Lá Oibre
Téarmaí Íocaíochta: T/T, L/C, Cárta Creidmheasa
Cumas Soláthair: 100000 Tonna in aghaidh na míosa
Deimhniú: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Easpórtáil chuig:

Stáit Aontaithe Mheiriceá, an India, Ceanada, an tSile, an Fhionlainn, Iosrael, an Iodáil, Cuáit, an Spáinn, an Ríocht Aontaithe, etc.

Comhdhéanamh Ceimiceach

Eilimint Carbón, C Cróimiam, Cr Nicil, Ni Mangainéis, Mn Sileacan, Si Fosfar, p Sulfar, S Nítrigin, N
                 
Ábhar (%) 0.04-0.10 18.0-20.0 8.0-10.5 Níos lú ná nó cothrom le 2.00 Níos lú ná nó cothrom le 0.75 Níos lú ná nó cothrom le 0.045 Níos lú ná nó cothrom le 0.030 Níos lú ná nó cothrom le 0.10

Airíonna Meicniúla

Maoin méadrach Impiriúil
     
Neart Teanntachta 515-860 MPa 74-125 ks
Neart Toradh 205-515 MPa 29.7-74 ks
Cruas Brinell (HB) 217-269 217-269
Cruas Rockwell (HRB)
Cruas Vickers (HV)
Fadú ag Sos 40-50% 40-50%
Modal Óg 193 GPa 28 msi

Glaoigh Linn