What is 1.4028 Stainless Steel?410 Stainless Steel Plate | Sheet304H Stainless Steel Sheet

Caighdeán

AMS 5659, AMS 5823, AMS 5862, ASTM A564 / A564M, ASTM A693

Grád

0Cr15Ni5Cu4Nb, 1.4545, S15500

Fad

1000 mm-6000 mm (39.37-236.22 in), Saincheaptha

Trastomhas

Barra: 6 mm-300 mm (0.24-12 in), Saincheaptha

Tinneas

Saincheaptha, Pláta: 6 mm-100 mm (0.24-3.94 in), Bileog: 0.5 mm-6 mm (0.02-0.24 in)

Leithead Iomlán

Saincheaptha, Bileog & Pláta: 1000 mm-2000 mm (39.37-78.74 in)

Críochnaigh Dromchla

2B, 2D, BA, Brataithe, srl., Talamh, Muileann, Uimh.1, Uimh.4, scafa, snasta, iompú

Foirm

15-Barra brionnaithe 5PH, 15-Pláta 5PH, pláta snasta 15-5PH, bileog 15-5PH, Bileog tempered 15-5PH, Coil, Barra Fuar Tarraingthe, Pláta Fuarrollta, srl., Barra Maol, Bileog te-rollta, Barra dronuilleogach, Slat, Barra Babhta, Barra Cearnóg

 

Comhdhúile Ceimiceacha

Cróimiam (Cr)Nicil (Ni)Copar (Cu)Mangainéis (Mn)sileacain (Si)Carbón (C)Fosfar (P)Sulfar (S)Nítrigin (N)
         
14.0 – 15.53.5 – 5.52.5 – 4.51.0 max1.0 max0.07 max0.04 uas0.03 max0.10 max

Airíonna Meicniúla

AiríonnaAonad MéadrachAonad Impiriúil
   
Neart Teanntachta1000-1170 MPa145-170 ksi
Neart Toradh≥ 1000 MPa≥ 145 ks
Cruas Vickers360 HV (tipiciúil)360 HV (tipiciúil)
Cruas Brinell350 HB (tipiciúil)350 HB (tipiciúil)
Cruas Rockwell35 HRC (tipiciúil)35 HRC (tipiciúil)
Fadú≥ 10%≥ 10%
Modal Leaisteacha200 GPa29.0 x 10³ ksi